post Oct 4 2009, 09:38 PM
Post #1


Member
*

Group: Members
Posts: 66
Joined: 28-September 09
Member No.: 28,329



What is the proper compound to use as a filler in the seams of the mahogany deck on my '46 Aristocrat?
Daddy
User is offlineProfile CardPM
Go to the top of the page
+Quote Post
fishcat
post Oct 5 2009, 09:28 PM
Post #2


Member
*

Group: Members
Posts: 52
Joined: 23-August 08
Member No.: 8,003



Take a look at sikaflex 291. I was researching that same question for my 59 Magellan. Unfortunately due to illness in family have not had a chance to test on a piece and then varnish.
User is offlineProfile CardPM
Go to the top of the page
+Quote Post

Reply to this topicStart new topic
2 User(s) are reading this topic (2 Guests and 0 Anonymous Users)
0 Members:

 



Lo-Fi Version Time is now: 9th September 2010 - 04:41 PM

The oPYnions expressed within the PY A&C BOC forum are those of their respective members,
not necessarily those of the club's membership as a whole. Your discretion is advised and appreciated

While we strive to ensure that individuals who offer items for sale or trade are legitimate,
the PY A&C BOC cannot/will not be held responsible for any monetary transactions or trades made via this Forum.